Stale ferrytyczne | |||||
N o r m y | EN 10088 | 1.4000 | 1.4003 | 1.4016 | 1.4510 |
PN Polska | 0H13 | - | H17 | 0H17T | |
AISI USA | 403,410S | - | 430 | 439 | |
DIN NIEMCY | X6Cr13 | X2CrNi12 | X6Cr17 | X3CrTi17 X6CrTi17 | |
S | C | <0.08 | <0.03 | <0.08 | <0.05 |
Si | <1.0 | <1.0 | <1.0 | <1.0 | |
Mn | <1.0 | <1.5 | <1.0 | <1.0 | |
P | <0.04 | <0.04 | <0.04 | <0.04 | |
S | <0.015 | <0.015 | <0.015 | <0.015 | |
N | - | <0.03 | - | - | |
Cr | 12.00-14.00 | 10.50-12.50 | 16.00-18.00 | 16.00-18.00 | |
Mo | - | - | - | - | |
Ni | - | 0.30-1.00 | - | - | |
Inne | - | - | - | Ti:4x(C+N)+0.15<0.80 |